AMS 5686 Superalloy Sheet Steel

  • 1
  • 2
  • 3

Brand Name : PANGANGGROUP,TISCO,ANSTEEL,BAOSTEEL

Model Number : AMS 5686

Certification : SGS, TUV, BV, ISO, MTC

Place of Origin : China

MOQ : 800kg

Price : Negotiations

Payment Terms : T/T

Supply Ability : 50000KGS/Month

Delivery Time : Ex-stock for delivery: 3-7 days Production lead time: 30-60 days

Packaging Details : Wooden Pallet BOX;Standard Seaworthy Package;based on the customer's special requirement

Product Name : AMS 5686 Superalloy Sheet Steel

Characteristic : Corrosion and Heat resisitant

Heat treatment condition : +N, +AT, etc

Processing methods : Peeld, Milled, etc

Available Shapes : Tubing, Steel plate, etc

Surface : Grinded, Bright, etc

Contact Now

AMS 5686 Superalloy Sheet Steel

Product Information

AMS 5686 steel has good high-temperature strength and oxidation resistance, and can operate for a long time without failure at high temperatures. Its high-temperature strength is higher than many other steels and can be used in high-temperature environments exceeding 1000 ℃. At the same time, AMS 5686 steel also has good corrosion resistance and superior performance when used in some chemically corrosive environments.


Size Range

Round bar / Wire rod (Diameter):1.0 mm to 1100 mm
Square bar / Flat bar: 1.0 mm to 1000 mm
Forging piece: Stepped shafts with flanks / discs /tubes /slugs /donuts /cubes /other different shapes based on OEM.
Heavy/middle plate via hot rolled: T5.0 - 1500 mm X W3 - 1000 mm X L100-1000 mm
Sheet steel via cold rolled: T1.0 - 10 mm X W1 - 1000 mm X L100 - 800 mm
Steel strip via cold rolled: T3.0 - 10 mm X W1.0 - 1500 mm X L (or in coil form)
Length: Fixed length or random length or based on the customer's special requirement.


Chemical Composition and standard

AMS 5686

Mechanical Properties

SAE AMS 5686G

C(%): ≤0.08
Si(%): ≤1.00
Mn(%): ≤2.00
P(%)≤: 0.03
S(%)≤: 0.025

Cr(%): 17.0~19.0
Ni(%): 10.0~13.0
Mo(%): ≤0.50

Cu(%): ≤0.50

Tensile strength,Rm/MPa: ≤758
Yield strength,Rp/MPa: -

Elongation, A/%: -

Reduction of area, ψ/%: -

Hardness HRC: -

AMS 5686 Superalloy Sheet Steel

Applications

AMS5686 is mainly used for manufacturing high-temperature mechanical components such as aviation engine components, turbine blades, and turbine discs


If you are interested in our products or have any questions, please contact our team of engineers at
sales@ss-bars.com


AMS 5686 Superalloy Sheet SteelAMS 5686 Superalloy Sheet Steel


AMS 5686 Superalloy Sheet Steel


Wholesale AMS 5686 Superalloy Sheet Steel from china suppliers

AMS 5686 Superalloy Sheet Steel Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: Mianyang Baoheng New Material Technology Co.,Ltd
*Subject:
*Message:
Characters Remaining: (0/3000)